Skip to main navigation Skip to search Skip to main content

Pitting Corrosion of 3D Printed 316 L Stainless Steel in Chloride and Hydrocarbon Environments

  • Ibrahim Albalawi

Student thesis: Master's Thesis

Date of Award3 May 2023
Original languageEnglish
SupervisorAhmad Sorour (Supervisor)

Cite this

'