A series of UV-protected coatings were prepared using cerium-oxide-functionalized oil fly ash (f-OFA-CeO2) in waterborne polyurethane (WBPU) dispersions. Three monomers, namely, poly(tetramethyleneoxide glycol) (PTMG), polydimethylsiloxane-hydroxy terminated (PDMS) and 4,4-dicyclohexylmethane diisocyanate (H12MDI), were used to pre-mix with f-OFA-CeO2 separately, followed by the synthesis of WBPU/f-OFA-CeO2 dispersions. The f-OFA-CeO2 distribution and enrichment into any part (top/bottom/bulk) of the coating was strongly affected by the pre-mixing of f-OFA-CeO2. The f-OFA-CeO2 was densely distributed in the top, bottom and bulk when the f-OFA-CeO2 was pre-mixed with PDMS, H12MDI and PTMG, respectively. Only an f-OFA-CeO2-enriched top surface showed excellent UV protection. The lowest UV-degraded exposed coating was found when the top surface of the coating was f-OFA-CeO2-enriched.

Original languageEnglish
Article number3232
JournalPolymers
Volume13
Issue number19
DOIs
StatePublished - 1 Oct 2021

Bibliographical note

Publisher Copyright:
© 2021 by the authors. Licensee MDPI, Basel, Switzerland.

Keywords

  • Coating
  • Degradation
  • Waterborne polyurethane

ASJC Scopus subject areas

  • General Chemistry
  • Polymers and Plastics

Fingerprint

Dive into the research topics of 'UV-protected polyurethane/F-oil fly ash-CeO2 coating: Effect of pre-mixing f -oil fly ash-CeO2 with monomers'. Together they form a unique fingerprint.

Cite this