Abstract
The aim of this study is to examine issues related to stress corrosion cracking (SCC) in nuclear power plants. The study will explore the relationship between materials and environmental variables which cause the onset and progression of SCC in different materials commonly used in piping systems and related infrastructure. SCC stands as a noteworthy concern within the nuclear power industry, resulting in expensive downtime and repair procedures, and carrying potentially severe safety implications. The findings of this study can provide insights into the mechanisms underlying SCC and inform the development of strategies for preventing and mitigating its effects on piping systems. By understanding the factors that contribute to SCC and how it can be mitigated, industries can develop strategies to prevent corrosion-related failures and ensure safe and reliable operation. The results of this study will contribute to the ongoing efforts to improve the reliability and safety of nuclear power plants and other industries that face similar corrosion-related challenges.
| Original language | English |
|---|---|
| Title of host publication | Challenges and Recent Advancements in Nuclear Energy Systems - Proceedings of Saudi International Conference on Nuclear Power Engineering SCOPE |
| Editors | Afaque Shams, Khaled Al-Athel, Iztok Tiselj, Andreas Pautz, Tomasz Kwiatkowski |
| Publisher | Springer Science and Business Media Deutschland GmbH |
| Pages | 296-308 |
| Number of pages | 13 |
| ISBN (Print) | 9783031643613 |
| DOIs | |
| State | Published - 2024 |
| Event | Saudi International Conference on Nuclear Power Engineering, SCOPE 2023 - Dhahran, Saudi Arabia Duration: 13 Nov 2023 → 15 Nov 2023 |
Publication series
| Name | Lecture Notes in Mechanical Engineering |
|---|---|
| ISSN (Print) | 2195-4356 |
| ISSN (Electronic) | 2195-4364 |
Conference
| Conference | Saudi International Conference on Nuclear Power Engineering, SCOPE 2023 |
|---|---|
| Country/Territory | Saudi Arabia |
| City | Dhahran |
| Period | 13/11/23 → 15/11/23 |
Bibliographical note
Publisher Copyright:© The Author(s), under exclusive license to Springer Nature Switzerland AG 2024.
Keywords
- Corrosion Mitigation; Reliability; Corrosion
- Nuclear Power Plant
- Stress Corrosion Cracking
ASJC Scopus subject areas
- Automotive Engineering
- Aerospace Engineering
- Mechanical Engineering
- Fluid Flow and Transfer Processes
Fingerprint
Dive into the research topics of 'Understanding Stress Corrosion Cracking (SCC), Affecting Variables and Prevention Strategies in Nuclear Power Plants-A Review'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver