Synthesis, Characterization, and Surface Analysis of Near-β Ti20Nb20Zr Alloy Proceeded by Powder Metallurgy for Biomedical Applications

Research output: Contribution to journalArticlepeer-review

9 Scopus citations

Fingerprint

Dive into the research topics of 'Synthesis, Characterization, and Surface Analysis of Near-β Ti20Nb20Zr Alloy Proceeded by Powder Metallurgy for Biomedical Applications'. Together they form a unique fingerprint.
Sort by

Engineering

Material Science