Research output: Patent
}
TY - PAT
T1 - Stress Corrosion Cracking Testing Device
AU - Rihan, Rihan
AU - Alhems, Luai
AU - Basapur, Mehaboob
PY - 2013
Y1 - 2013
M3 - Patent
M1 - US8474324
ER -