Abstract

A method for producing a submicron-/nano-jute carbon/epoxy composite anti-corrosion coating is described. The method includes heating a jute stick, grinding the jute stick to form a first powder; pyrolyzing the first powder to form a pyrolyzed carbon; grinding the pyrolyzed carbon to form a second powder; ball milling the second powder under the wet conditions to form a submicron-/nano-jutecarbon; mixing the submicron-/nano-jutecarbon, and an epoxy resin to form a first mixture; mixing a hardener with the first mixture to form a second mixture, and coating the second mixture on a mild steel substrate and curing to form the submicron-/nano-jutecarbon/epoxy composite anti-corrosion coating.