Corrosion study of SS304 and SS316 alloys in atmospheric, underground and seawater splash zone in the Arabian Gulf

Research output: Contribution to journalArticlepeer-review

37 Scopus citations

Abstract

Bare stainless steel type 304 and 316 alloys were exposed to atmospheric, underground and seawater splash conditions in order to evaluate their corrosion properties. The exposure was undertaken for 15 months at the coastal and industrial city of Jubail located in the Arabian Gulf. The corrosivity of the environment was determined by testing the soil, groundwater, seawater and air quality. Corrosion rate of the exposed coupons was determined by weight loss method. The experimental results indicate that the both types of stainless steels corroded moderately in this environment. Primary factors influencing the corrosion process are thought to be high degree of variation in temperature and humidity combined with high chloride and sulphate concentrations. The corrosion rate of stainless steel is also compared with those reported for other international locations.

Original languageEnglish
Pages (from-to)134-140
Number of pages7
JournalCorrosion Engineering Science and Technology
Volume52
Issue number2
DOIs
StatePublished - 17 Feb 2017

Bibliographical note

Publisher Copyright:
© 2017 Institute of Materials, Minerals and Mining Published by Taylor & Francis on behalf of the Institute.

UN SDGs

This output contributes to the following UN Sustainable Development Goals (SDGs)

  1. SDG 11 - Sustainable Cities and Communities
    SDG 11 Sustainable Cities and Communities

Keywords

  • SS304
  • SS304
  • SS316
  • atmospheric
  • corrosion
  • splash zone
  • underground

ASJC Scopus subject areas

  • General Chemistry
  • General Chemical Engineering
  • General Materials Science

Fingerprint

Dive into the research topics of 'Corrosion study of SS304 and SS316 alloys in atmospheric, underground and seawater splash zone in the Arabian Gulf'. Together they form a unique fingerprint.

Cite this