Coarse-grained superplasticity of a Ni-Co-based superalloy

  • Rashad A. Al-Hammadi
  • , Rui Zhang*
  • , Chuanyong Cui
  • , Zijian Zhou
  • , Yizhou Zhou
  • *Corresponding author for this work

Research output: Contribution to journalArticlepeer-review

4 Scopus citations

Abstract

A near-superplastic tensile elongation of up to 232% at 1140 °C and 0.001 s−1 for a coarse-grained Ni-Co-base superalloy with an average grain size of 85 µm is reported. Nevertheless, poor grain deformation coordination and low grain boundary bonding strength led to terrible thermoplasticity for the coarse-grained alloy below 1100 °C. Dynamic recrystallization (DRX) relieved the stress concentration and decreased the damage accumulation during superplasticity, improving the ductility with the increase in temperature within the γ + γ′ dual-phase regime.

Original languageEnglish
Article number135263
JournalMaterials Letters
Volume353
DOIs
StatePublished - 15 Dec 2023

Bibliographical note

Publisher Copyright:
© 2023 Elsevier B.V.

Keywords

  • Coarse grains
  • Metal and alloys
  • Microstructure
  • Ni-Co-based superalloy
  • Superplasticity

ASJC Scopus subject areas

  • General Materials Science
  • Condensed Matter Physics
  • Mechanics of Materials
  • Mechanical Engineering

Fingerprint

Dive into the research topics of 'Coarse-grained superplasticity of a Ni-Co-based superalloy'. Together they form a unique fingerprint.

Cite this